Perkin Elmer DSC-7 Differential Scanning Calorimeter Differential Scanning Calorimeter (DSC)

Model: 
DSC-7 Differential Scanning Calorimeter
Manufacturer: 

The Perkin-Elmer DSC-7 differential scanning calorimeter is used to accurately measure melting points, glass transitions, and heats of fusion. Typical temperature range is from 10 C to 400 C. The temperature scale is calibrated using a two-point calibration, measuring the onset temperatures of indium and zinc standards. The enthalpy scale is calibrated using the observed delta-H from an accurately known amount of indium.